Make Iron Oxide

Iron is a crucial metal in our world. It fuels the steel industries and allows blood to carry oxygen to our cells. It comes as no surprise that iron containing compounds are of great interest. One such group of these compounds, called iron oxides, is formed by reacting iron and oxygen in some way. Which oxide you get depends on the specific circumstances under which the iron and oxygen react, and this will change the properties and uses of the resulting iron oxide.

Steps

Making Iron (II,III) Oxide (Magnetite)

  1. Locate a source of iron (III) (iron in the 3+ oxidation state). An iron (III) salt such as ferric chloride will be easy to add to solution.It is often used for etching copper, so you can buy it online, at a chemical supply store, and sometimes even an electronics store such as RadioShack Also, a fine rust powder would work well. You can collect rust and grind it to a fine powder, if you choose to go that route.[1]
  2. Make a solution containing iron (III). Add water to the iron (III) oxide source in a beaker (or other container). The aqueous environment (in water) is ideal for the iron (III) and iron (II) molecules to react with each other and with oxygen. It will suspend your iron (III) molecules in solution and make it easy to combine with the iron (II) and oxygen molecules. You do not need to cover the container, but this can help keep out contaminants. [1]
  3. Locate a source of iron (II) (iron in the 2+ oxidation state). Since iron (II) in its pure form is rare under atmospheric conditions, you will likely need to use an iron (II) salt. Iron sulphate, iron (II) chloride, and iron (II) phosphate are relatively common options. Iron sulphate is used in gardening and can be found at most garden supply stores.[1]
  4. Make a solution containing iron (II). Whatever your choice of iron (II) salt, you will need to dissolve it in water. Do this as a separate beaker (or other container) from the iron (III) solution to ensure that the iron (III) has not saturated the water. This will allow the most iron (II) to dissolve into the water. Again, a lid will help keep out contaminants, but is not necessary.[1]
  5. Mix the solutions. Combine the iron (III) solution and the iron (II) solution into the same container. This will allow bring the iron (III) ions and the iron (II) ions into contact with each other. They will also contact oxygen in the water and the atmosphere, which is needed to produce magnetite.[1]
  6. Oxidize the solution. While the reaction will proceed by mixing the two solutions together, it will proceed very slowly. You can speed up the reaction by adding an oxidizing solution, such as ammonia. Hydrogen peroxide is also a good oxidizing agent.[1]
    • The addition of an oxidizing agent will allow the reaction to proceed much faster. Times will vary based on the ratios of reactants and oxidizer, but you will likely see some change in just a few seconds.
    • Storing your iron oxide in a dry place is recommended.

Making Iron (III) Oxide (Rust) Using Electrolysis

  1. Obtain a source of iron. Aside from some salts, most iron compounds tend to be in the iron (III) state. This includes things like railroad ties, nails, steel wool, paperclips, etc. Choose your source based on the amount of iron you need, how fast you need it, and what is available to you. For example, steel wool is cheap and oxidizes quickly, but railroad ties contain a larger mass of iron.[2]
  2. Fill a container with water. You want to be sure that you have enough water in the container to cover the iron piece at all times. Keep in mind that the process of electrolysis may heat the water. This can increase the rate at which the water evaporates.[3]
  3. Find a power source. You will need to use a battery or other direct current power source to power the reaction. The power source should have a lead connected to the negative side and a lead to the positive side. Choose the size of your power source based on how much rust you are trying to create and how fast you want it. Larger power supplies will generally create rust faster.[3]
  4. Submerge the positive and negative leads. The leads should not touch each other. Instead, they should be submerged in opposite sides of your water tank. This will make the water solution part of the circuit and force electricity to flow through the water.[3]
  5. Submerge your iron source. While iron will typically rust under atmospheric conditions without any help, submerging it in water increases the rate of oxidation. Submerging iron in water that is being electrolyzed will increase the rate of oxidation even more since the electrolysis produces hydrogen gas (H2) and diatomic oxygen (O2). Diatomic oxygen is a great oxidizer and readily reacts with the iron to form rust.[3]
  6. Turn on the power. Now that your tank is setup, you can turn on the power. This will start the current flowing through the solution and oxidizing the metal. Be careful not to touch the leads, or touch them together. Also, do not put your hands in the water unless you turn the power off.
    • If you are using a power source without a switch (like a battery), either put the leads in last, or do not hook the leads to the battery until you are ready for power.
  7. Allow to sit. While the reaction is relatively fast compared to natural oxidation, it isn’t instant. You will need to leave the reaction for several hours at least to yield rust. You will probably need to leave it for a day or two to get a decent amount.[3]
  8. Filter the solution. When your rust forms, it will be in the tank of water. The first step to getting it in a dry and usable form is to filter out some of the water. You can stretch cheesecloth or some other fabric over a jar or sink and pour the solution through. Allow it to sit for an hour or so to drain as much water as possible.[3]
  9. Dry the resulting rust. To finish drying your rust, you will need to bake it. Set your oven at 400 degrees Fahrenheit and bake the rust for one to three hours. Be sure to use an old pan, the rust will stain it.[3]

Making Iron (III) Oxide (Rust) Using a Strong Oxidizer

  1. Choose an iron source to oxidize. The more exposed surface area your source has, the better. For example, steel wool has a lot of surface area relative to its size, while a railroad tie has much less. Your oxidizer can only act on the surface of your iron.[2]
  2. Choose an oxidizing agent. Bleach is a great oxidizing agent. Another good choice is hydrogen peroxide. A weaker oxidizing agent is salt water. The oxidizer you choose will determine how fast the iron is oxidized. The stronger your oxidizing agent, the faster your iron will oxidize.[2]
  3. Expose the iron source to the oxidizer. You can submerge the iron source in the oxidizing solution. Another option is to spray the oxidizer on the iron at regular time intervals (every hour or so). Depending on how fast you want the reaction to proceed and how comfortable you are using strong oxidizers, you can dilute the oxidizer in water (this will weaken it and slow the reaction).[2]
  4. Allow the reaction to proceed. Depending on your choice of oxidizer and exposure, this can take several hours or several days. You should certainly start to see rust forming within a week. If not, check to make sure you are using iron and that it is not coated with a protective layer such as wax.[2]
  5. Collect and dry the resulting rust. You may have to scrape the rust off the surface of your iron piece to collect it. If you submerged the piece, you can filter the rust from the solution. If your rust is wet, dry it in an oven at 400 degrees Fahrenheit for one to three hours.[2]

Making Iron (II) Oxide (Black Rust) by Burning Steel Wool

  1. Find a piece of plain steel wool. If the wool has any rust inhibitors or soaps on it, it will interfere with your results. You should also look for a steel wool with thin fibers. This will make it easier for the fibers to ignite and burn.[4]
  2. Place the steel wool on a fireproof surface. You will not be able to hold the steel wool in your hand. It will be on fire! You also do not want to burn anything down. Glass plates or tin lids are great choices.[4]
  3. Use a 9-V battery to ignite the steel wool. Touching a 9-V battery to the steel wool will connect the positive and negative leads of the battery. This closes the circuit and allows electricity to flow. The steel wool will ignite because more current is flowing through than it can handle, so it heats up until it reaches an ignition point.[4]
  4. Observe the black rust that is formed. Black rust is formed as a result of oxidation in an oxygen deprived environment. Since the steel wool is oxidized so rapidly in this reaction there is little time for enough oxygen to access the iron to form iron (III) oxide (red rust).[4]

Tips

  • You can use iron oxide as pigment, to buff jewelry, or to make thermite.
  • You should use a benchtop or other work surface for any of these experiments. Stains and damage to the work surface are likely to occur.
  • Wear a ventilator to protect your lungs.

Warnings

  • Always wear goggles.
  • Always wear gloves.
  • Handle all chemical reactions, especially the oxidizers, with care.
  • Mixing bleach with acids will produce toxic gas.

Things You’ll Need

  • Piece of Iron
  • Oxidizing Agent
  • Water
  • Filter
  • Water Containers
  • Power Source

Related Articles

Sources and Citations

You may like